Ore-formation process simulation
Simulate the migration, metasomatism and mineral precipitation of ore-bearing hydrothermal fluids through host rock, and study the mechanisms of element transport, enrichment and spatial zonation.
A batch-experiment platform for ore-formation simulation and high-pressure high-temperature water-rock reaction. 300MPa maximum working pressure, 850℃ maximum operating temperature, with magnet-ring quench, pressure-hold leak testing and programmed pressure-temperature curves under full-process control. Single-unit customisation and multi-unit parallel operation are supported.
The GS850 cold-seal autoclave ore-formation simulation system is developed and manufactured by Hubei Guangshi Precision Co., Ltd. It reproduces the temperature and pressure conditions of low-to-medium temperature hydrothermal environments in the laboratory, for ore-formation process simulation, water-rock reaction and long-duration constant-temperature experiments. The system uses a cold-seal vessel structure: the vessel carries the pressure while the furnace controls temperature independently. The cap is tightened with a torque wrench to a set value (≥80 N·m), and the double-cone sealing faces deliver 300MPa-class closure.
The system is equipped with a magnet-ring quench mechanism: at the end of an experiment, pulling the magnet ring moves the sample rack to the cold zone in one motion. A pressure rise of 40–50MPa confirms a successful quench, so samples can be quenched rapidly without breaking the seal, preserving intermediate reaction states.
| Item | Specification | Notes |
|---|---|---|
| System name | GS850 cold-seal autoclave ore-formation simulation system | Unit numbering SB-SR-001~010 |
| Maximum working pressure | 300MPa | As marked on the equipment nameplate |
| Maximum operating temperature | 850℃ | As marked on the equipment nameplate |
| Sealing structure | Cold-seal · double-cone seal | Cap torque ≥80 N·m; hose 16–20 N·m (18 N·m recommended) |
| Pressure-hold leak test | 30–60 min · fluctuation ≤2MPa | Less than 30 min is not enough to expose micro-leaks |
| Pre-heating depressurisation | ≥1/4 of the experimental pressure | Prevents overpressure from thermal expansion on heating; alternatively depressurise fully and re-pressurise |
| Daily inspection criterion | Pressure drop ≤1%/24h is normal | A drop ≥1MPa within 1h indicates an abnormal leak |
| Leak detection | With fluid: bake at 120℃ for 2h and weigh Without fluid: immerse in alcohol for 2h and weigh | Any weight change means a leak; do not put into service |
| Quench method | Magnet-ring quench | A pressure rise of 40–50MPa confirms success; no rise means failure |
| Depressurisation temperature limit | <100℃ | Above 100℃, opening valves to depressurise or disassembling is strictly prohibited |
| Cooling method | Forced cooling by circulating water chiller | Must run continuously throughout the entire heating phase |
| Run control | Programmed pressure-temperature curves | Multi-segment heating and soaking programmes, logged run by run |
The GS850 is governed by both the GS850 Equipment Experiment Operating Procedure and the quick-start manual. The core discipline is check water first, check the station second, never heat without a passed pressure hold, never touch a wrench above 100℃:
Simulate the migration, metasomatism and mineral precipitation of ore-bearing hydrothermal fluids through host rock, and study the mechanisms of element transport, enrichment and spatial zonation.
Study rock alteration, dissolution–precipitation equilibrium and element transport rates under long-duration high-pressure high-temperature conditions.
Study hydrogen generation from supercritical water–rock interaction, supported by the methodology of our hydrogen-generation simulation white paper.
Evaluate the corrosion behaviour and service life of alloys, coatings and sealing materials in high-pressure high-temperature aqueous environments.
The GS850 is available in two cooperation modes: complete-unit purchase and contract experiment services. Contract experiments are billed at ¥50 per machine-hour; pressure-temperature programmes are tailored to your project, and experiment records and samples are delivered with the order:
Pull the magnet ring to move the sample rack to the cold zone in one motion. A pressure rise of 40–50MPa confirms a successful quench; no rise means the quench failed. The seal stays intact throughout, so intermediate reaction states are preserved.
Micro-leaks take time to show up. A hold shorter than 30 minutes is not sufficient to expose them. The hold passes only when fluctuation stays within 2MPa over 30–60 minutes; otherwise the vessel must be depressurised, the cone sealing faces and fittings inspected, and the test repeated.
During routine inspection, a pressure drop of ≤1%/24h is normal; a drop ≥1MPa within 1h indicates an abnormal leak. For a definitive check: with fluid inside, bake at 120℃ for 2h and weigh; without fluid, immerse in alcohol for 2h and weigh — any weight change means a leak and the vessel must not be used.